Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.60e+10 ohm-cm @Temperature 112 °C |
7.60e+10 ohm-cm @Temperature 234 °F |
cured 2 hours @ 93°C |
Abatron AboCast 50-3/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |