Comparative Tracking Index 450 V

@Thickness 3.20 mm
450 V

@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
Comparative Tracking Index 450 V

@Thickness 3.20 mm
450 V

@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66
Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..