Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond F202 Anaerobic Retainer
The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond HL126 Anaerobic Threadlocker
PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond HM118 Anaerobic Threadlocker
Permabond® HM118 Threadlocker is an excellent general-purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Cure is fast and reliable on s..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond HM128 Anaerobic Threadlocker
Permabond® HM128 Threadlocker is a high strength adhesive for permanent assembly. It is typically used for preventing vibration loosening of bolts, studs and cap screws. Full cure to a cross-linked..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond HM160 Anaerobic Retaining Compound
Permabond® HM160 is a medium viscosity liquid adhesive that cures when confined between metal parts to form a tough, hard plastic. In the uncured, liquid state, the adhesive wets the metal surfaces..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond HM165 Anaerobic Retainer
Permabond® HM165 is a high viscosity anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It is best suited for cylindrical parts and where high temperatu..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond F201 Anaerobic Retainer
Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond HH040 Anaerobic Retainer
Permabond® HH040 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure unitiz..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond HH040 Pure NSF 61 Approved Anaerobic Retainer
Permabond® HH040 PURE is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure u..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond MM115 Anaerobic Threadlocker
Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance...
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond MM115P Pure Anaerobic Threadlocker
Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten..
Cure Time 4.98 - 9.60 min

@Temperature 149 °C
0.0830 - 0.160 hour

@Temperature 300 °F
Master Bond Supreme 3HT High Bond Strength One Component Epoxy Adhesive System
Master Bond Polymer System Supreme3HT is a storage stable one component, heat curing epoxy adhesive featuring a hither to unattainable balance of performance properties including both high shear and..
Cure Time 4.98 - 10.0 min

@Temperature 149 °C
0.0830 - 0.167 hour

@Temperature 300 °F
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive
Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt..
Cure Time 4.98 - 10.0 min

@Temperature 149 °C
0.0830 - 0.167 hour

@Temperature 300 °F
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive
Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic..
Cure Time 4.98 - 9.60 min

@Temperature 149 °C
0.0830 - 0.160 hour

@Temperature 300 °F
Master Bond EP3HT Fast Curing One Component Epoxy System
Master Bond Polymer System EP3HT is a one component system featuring high shear strength and good temperature resistance along with a fast cure schedule. Master Bond Polymer System EP3HT produces du..
Cure Time 4.98 - 9.60 min

@Temperature 149 °C
0.0830 - 0.160 hour

@Temperature 300 °F
Master Bond EP3HTMED One Component, Biocompatible Epoxy System
Master Bond Polymer System EP3HTMed combines the ease of a one part, no mix, fast curing adhesive with high shear strength. This special formulation fully meets USP Class VI requirements. EP3HTMed p..
Cure Time 4.98 min

@Temperature 75.0 °C
0.0830 hour

@Temperature 167 °F
Dust Free, at 50% humidity
Blue River Coatings Acrylic 4000D Topcoat
BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo..
Cure Time 4.98 min

@Temperature 75.0 °C
0.0830 hour

@Temperature 167 °F
Recoat, at 50% humidity
Blue River Coatings Semi-Transparent Wood Stain Concentrate
BLUE RIVER COATINGS Semi-Transparent Wood Stain is a water based stain developed to provide long lasting protection and a beautiful appearance on wood surfaces. BLUE RIVER COATINGS Semi-Transparent ..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond A011 Anaerobic Threadlocker
Permabond® A011 is an anaerobic adhesive designed for locking and sealing threaded or coaxially fitting metal parts where subsequent dismantling is required. Its controlled strength ensures fatigue..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond A1042 Anaerobic Threadlocker
Permabond® A1042 is a rapid curing adhesive designed to lock and seal metal parts that subsequently may need to be dismantled for maintenance. The high vibration resistance makes Permabond A1042 pa..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond A1042 Anaerobic Threadlocker
Permabond® A1042 is a rapid curing adhesive designed to lock and seal metal parts that subsequently may need to be dismantled for maintenance. The high vibration resistance makes Permabond A1042 pa..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond A1044 Anaerobic Threadsealant
Permabond® A1044 is a rapid curing sealant designed to lock and seal metal pipe connections, offering very good resistance to even the most aggressive chemicals. Permabond A1044 can be used to seal..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond HM135 Anaerobic Retainer
Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras..
Cure Time 4.98 - 10.2 min

@Temperature 23.0 °C
0.0830 - 0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond HM135 Anaerobic Retainer
Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras..
Cure Time 4.98 - 10.2 min

@Temperature 23.0 °C
0.0830 - 0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond A1046 Anaerobic Retainer
Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and ..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond A126 Anaerobic Retainer
Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u..
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
Permabond A136 Anaerobic Gasketmaker
Permabond® A136 is an anaerobic material designed for making 'formed in situ' gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets thereby offering potent..
Cure Time 4.98 min

@Temperature 75.0 °C
0.0830 hour

@Temperature 167 °F
Dust Free, at 50% humidity
Blue River Coatings Acrylic 4000 Topcoat
BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo..