3M 3104 Polyethylene Protective Tapes

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 3104 Polyethylene Protective Tapes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Polyethylene Protective Tapes 3104 has a low-tack adhesive system to help provide temporary protection of many polished metals, smooth plastics, glass materials and high gloss painted surfaces.Information provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.70 MPa
247 psi
ASTM D3759
Elongation at Break 450 %
450 %
ASTM D3759
Peel Strength 0.0110 kN/m
0.0625 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Clear