Polymer Property : Peel Strength = 0.0110 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.0110 kN/m
0.0625 pli
Adhesion to Steel; ASTM D3330
3M 1614 Polyester Protective Tape
3M™ Polyester Protection Tape 1614 is a polyester tape with a low-tack adhesive system for temporary surface protection.Information provided by 3M
Peel Strength 0.0110 kN/m
0.0625 pli
Adhesion to Steel; ASTM D3330
3M 2104 Polyethylene Protective Tapes
3M™ Polyethylene Protective Tapes 2104 has a very low-tack adhesive system to helpInformation provided by 3M
Peel Strength 0.0110 kN/m
0.0625 pli
Adhesion to Steel; ASTM D3330
3M 21804 Industrial Polyethylene Temporary Surface Protection Tape
3M™ Industrial Polyethylene Temporary Surface Protection Tape 21804 is a very low adhesion temporary protection tape designed for a variety of surface protection applications.Information provided b..
Peel Strength 0.0110 kN/m
0.0625 pli
Adhesion to Steel; ASTM D3330
3M 2A04 Co-Extruded Polyethylene Protective Tapes
3M™ Co-Extruded Polyethylene Protective Tapes have a low-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M
Peel Strength 0.0110 kN/m
0.0625 pli
Adhesion to Steel; ASTM D3330
3M 3104 Polyethylene Protective Tapes
3M™ Polyethylene Protective Tapes 3104 has a low-tack adhesive system to help provide temporary protection of many polished metals, smooth plastics, glass materials and high gloss painted surfaces...
Peel Strength 0.0110 kN/m
0.0625 pli
Adhesion to Steel; ASTM D3330
3M 31804 Industrial Polyethylene Temporary Surface Protection Tape
3M™ Industrial Polyethylene Temporary Surface Protection Tape 31804 is a very low adhesion temporary protection tape designed for a variety of surface protection applications.Information provided b..
Peel Strength 0.0110 kN/m
0.0625 pli
Kraft Paper, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
3M 7142 Repositionable Paper Label Material
3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly f..
Peel Strength 0.0110 kN/m
0.0625 pli
Corrugated Board, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
3M 7142 Repositionable Paper Label Material
3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly f..
Peel Strength 0.0110 kN/m
0.0625 pli
Kraft Paper, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
3M 7142 Repositionable Paper Label Material
3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly f..
Peel Strength 0.0110 kN/m
0.0625 pli
Corrugated Board, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
3M 7142 Repositionable Paper Label Material
3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly f..
Peel Strength 0.0110 kN/m
0.0625 pli
Kraft Paper, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
3M 7113 Repositionable Paper Label Material
3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly f..
Peel Strength 0.0110 kN/m
0.0625 pli
Corrugated Board, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
3M 7113 Repositionable Paper Label Material
3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly f..
Peel Strength 0.0110 kN/m
0.0625 pli
Kraft Paper, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
3M 7113 Repositionable Paper Label Material
3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly f..
Peel Strength 0.0110 kN/m
0.0625 pli
Corrugated Board, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
3M 7113 Repositionable Paper Label Material
3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly f..