3M 415 Splicing Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 415 Splicing Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M
Physical Properties Metric English Comments
Thickness 102 microns
4.00 mil
Release Liner
102 microns
4.00 mil
Tape Only
Mechanical Properties Metric English Comments
Peel Strength 0.27391 kN/m
1.5625 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 65.0 °C
149 °F
Long term
82.0 °C
180 °F
Short term
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Carrier Polyester Film
Adhesive Type 400
Appearance Clear
Liner Tan 60# Densified Kraft