3M 4604 Silicone Rubber Termination Kit

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 4604 Silicone Rubber Termination Kit.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ 4604 and 4605 Quick Term II Silicone Rubber Termination Kits are three-piece Cold Shrink terminations for Tape Shield, Wire Shield, and LC Shield power cables. They meet the requirements of IEEE standard 48-1990, for class 1 terminations. In addition they meet German standard VDE 0278 parts 5 & 100, British standard BS C-89, Spanish standard UNE 21-115-75 and Brazilian standard A-B-N-T-9314. Similar terminations using Quick Term II technology meet French EdF standards HN 33-E-01 and HN 41-E-01. Data on foreign standards are available upon request. The 3M Quick Term II consists of a high dielectric constant (High-K) stress control tube insulated with a molded silicone skirted insulator. The 4600-series termination is a twelve-skirt design incorporating in one-piece base termination assembly, a four-skirt extension insulator, and a Silicone Rubber Jacket-Sealing Cold Shrink PST Assembly. Quick Term II terminations are provided in an expanded state; mounted on a removable inner supporting plastic core. As supplied in this pre-stretched condition and termination is ready for field installation. During installation the core in unwound, allowing the termination to shrink and form a tight seal. Collectively, these termination kits cover cables with primary insulation O.D. from 1.31” to 2.60” (33 to 66 mm). These kits can be used to terminate 46 kV Shielded Power Cables from 4/0 AWG to 1500 kcm.Information provided by 3M
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.27 MPa
1200 psi
Silicone Rubber Insulator; ASTM D42-68
9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42-68
Electrical Properties Metric English Comments
Dielectric Constant 2.7

@Temperature 130 °C
2.7

@Temperature 266 °F
Silicone Rubber Insulator; ASTM D150-70
3.0

@Temperature 90.0 °C
3.0

@Temperature 194 °F
Silicone Rubber Insulator; ASTM D150-70
3.4

@Temperature 23.0 °C
3.4

@Temperature 73.4 °F
Silicone Rubber Insulator; ASTM D150-70
20

@Frequency 100000 Hz
20

@Frequency 100000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
24

@Frequency 10000 Hz
24

@Frequency 10000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
29

@Frequency 1000 Hz
29

@Frequency 1000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
35

@Frequency 150 Hz
35

@Frequency 150 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
24.5

@Frequency 60.0 Hz,
Temperature 65.0 °C
24.5

@Frequency 60.0 Hz,
Temperature 149 °F
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
25.2

@Frequency 60.0 Hz,
Temperature 90.0 °C
25.2

@Frequency 60.0 Hz,
Temperature 194 °F
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
25.7

@Frequency 60.0 Hz,
Temperature 23.0 °C
25.7

@Frequency 60.0 Hz,
Temperature 73.4 °F
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
27.2

@Frequency 60.0 Hz,
Temperature 65.0 °C
27.2

@Frequency 60.0 Hz,
Temperature 149 °F
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
27.7

@Frequency 60.0 Hz,
Temperature 90.0 °C
27.7

@Frequency 60.0 Hz,
Temperature 194 °F
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
28.8

@Frequency 60.0 Hz,
Temperature 23.0 °C
28.8

@Frequency 60.0 Hz,
Temperature 73.4 °F
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
Dielectric Strength 20.0 kV/mm

@Thickness 0.190 mm
507 kV/in

@Thickness 0.00750 in
Silicone Rubber Insulator; ASTM D149-70
Dissipation Factor 0.12

@Frequency 100000 Hz
0.12

@Frequency 100000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
0.14

@Frequency 10000 Hz
0.14

@Frequency 10000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
0.15

@Frequency 1000 Hz
0.15

@Frequency 1000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
0.16

@Frequency 150 Hz
0.16

@Frequency 150 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
0.093

@Thickness 1650 mm,
Frequency 60.0 Hz
0.093

@Thickness 65.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
0.096

@Thickness 584 mm,
Frequency 60.0 Hz
0.096

@Thickness 23.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
0.132

@Thickness 2290 mm,
Frequency 60.0 Hz
0.132

@Thickness 90.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
0.161

@Thickness 2290 mm,
Frequency 60.0 Hz
0.161

@Thickness 90.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
0.165

@Thickness 1650 mm,
Frequency 60.0 Hz
0.165

@Thickness 65.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
0.166

@Thickness 584 mm,
Frequency 60.0 Hz
0.166

@Thickness 23.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
Track Resistance 36000 sec
36000 sec
2.5 kV, 10 k Ohms; ASTM 2303-68