Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.0 kV/mm | 508 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 6 FRC 2 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization FeaturesLongterm external use is possible because of the material stabilization with the light stabilizers on the HALS basis. Meets the flammability in accordance with the norm DIN 4102 - B1. PA 6.. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 6 GF 30 TS Polyamide 6, 30% Glass Fiber, Thermal Stabilization FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, heat stabilized, mouldings resistant against long-time heat impact up to 150°C. Decrease in tensile strength by 50%.. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 6 GF 35 Polyamide 6, 35% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 35% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 3.20 mm |
508 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 3.20 mm |
508 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® PPC4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | IEC 60243-1 |
DSM Akulon® S223-TP4 Impact Modified Nylon 66 (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D-149 |
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha.. |
|||
Dielectric Strength | >= 20.0 kV/mm | >= 508 kV/in | Superior Quality |
Kazanorgsintez PC-005 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | 4kV/s; ASTM D149 |
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha.. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D149/DIN 53481 |
Kolon KOPA® KN173HI4 High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D149 |
Kotec Carbotex KG-20MRA Polycarbonate, 20% Glass Fiber Reinforced Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D149 |
Kotec Carbotex KG-30F15 Polycarbonate, Wear Resistant, 30% Glass Fiber Reinforced Features: Glass fiber 30% reinforced, Mold release, Translucent, Dimensional stability, Non-frictionApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation p.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 2.00 mm |
508 kV/in @Thickness 0.0787 in |
ASTM D149 |
Gromax PBT 4130-201D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | |
Momentive Performance Materials RTV167 Gray Adhesive Sealant, Non-Corrosive High Strength One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Highest strength ad.. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D149/DIN 53481 |
Kolon Kopa® KN133 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Dielectric Strength | >= 20.0 kV/mm @Thickness 2.00 mm |
>= 508 kV/in @Thickness 0.0787 in |
ASTM D149 |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Dielectric Strength | >= 20.0 kV/mm @Frequency 50.0 Hz |
>= 508 kV/in @Frequency 50.0 Hz |
ASTM D149 |
Iran Petrochemical (PCC) PC 1822 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm |
508 - 635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 3.20 mm |
508 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East) 50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | |
Shin-Etsu Silicones KE-200 Silicone, Potting/Encapsulation RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | IEC 243; DIN 53481 |
Zell-Metall Engineering Plastics Zellamid 1500 (PEEK) Zellamid® 1500 (Polyetheretherketone - PEEK, natural) is the registered trademark for Zell-Metalls semi-crystalline high performance thermoplastic which exhibits a unique combination of high m.. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D-149 |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | IEC 60243-1 |
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | IEC 60243-1 |
DSM Arnitel® PL381 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 3.20 mm |
508 kV/in @Thickness 0.126 in |
Short time; ASTM D149 |
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 3.20 mm |
508 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Eurostar Staramide BG6 PA6, 30% Glass Filled, Injection Molded BG6 is a 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 1.00 mm |
508 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 2.00 mm |
508 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® 301-G20 PBT Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 20.0 - 30.0 kV/mm | 508 - 762 kV/in | Average value: 25.0 kV/mm Grade Count:14 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 2.00 mm |
508 kV/in @Thickness 0.0787 in |
ASTM D149 |
Chang Chun Plastic PBT2000 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |