3M 4H83W Protective Laser Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 4H83W Protective Laser Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Protective Laser Tape 4H83 is a clear or white multi-polymer film coated with medium-tack adhesive designed especially to help provide temporary protection of #3 & #4 stainless steel sheets during laser cutting and apply easily to the metal surfaces using roll pressure lamination.Information provided by 3M
Physical Properties Metric English Comments
Thickness 102 microns
4.00 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.1 MPa
3500 psi
ASTM D3759
Elongation at Break 750 %
750 %
ASTM D3759
Peel Strength 0.1205 kN/m
0.6875 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Custom
Appearance Clear, White