Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 7951 Hi-Performance Acrylic 300MP

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7951 Hi-Performance Acrylic 300MP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This adhesive is designed for applications requiring greater initial adhesion especially to low surface energy (LSE) plastic substrates. Temperature performance is up to 300°F (149°C) for most applications.Double-linered 300MP. High bond strength to low surface energy plastics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Adhesive
Mechanical Properties Metric English Comments
Shear Strength 0.531 MPa
77.0 psi
Cohesion Dynamic, PET/Polycarbonate; ASTM D1002
0.655 MPa
95.0 psi
Cohesion Dynamic, PET/Stainless Steel; ASTM D1002
Peel Strength 0.40538 kN/m
2.3125 pli
90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330
0.40538 kN/m
2.3125 pli
90° Peel, PET/PET, Initial (20 mins); ASTM D3330
0.44921 kN/m
2.5625 pli
90° Peel, PET/Polycarbonate, Initial (20 mins); ASTM D3330
0.51494 kN/m
2.9375 pli
90° Peel, PET/Aluminum, Initial (20 mins); ASTM D3330
0.62451 kN/m
3.5625 pli
90° Peel, PET/Polycarbonate, 72 hrs at RT; ASTM D3330
0.64642 kN/m
3.6875 pli
90° Peel, PET/PET, 72 hrs at RT; ASTM D3330
0.66833 kN/m
3.8125 pli
90° Peel, PET/Aluminum, 72 hrs at RT; ASTM D3330
0.77789 kN/m
4.4375 pli
90° Peel, PET/Polycarbonate, 72 hrs at 70°C; ASTM D3330
0.84363 kN/m
4.8125 pli
90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330
0.84363 kN/m
4.8125 pli
90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330
0.964 kN/m
5.50 pli
90° Peel, PET/Aluminum, 72 hrs at 70°C0; ASTM D3330
1.0408 kN/m
5.9375 pli
90° Peel, PET/Stainless Steel, 72 hrs at 70°C; ASTM D3330
Thermal Properties Metric English Comments
CTE, linear 4.90 µm/m-°C

@Temperature 27.0 - 175 °C
2.72 µin/in-°F

@Temperature 80.6 - 347 °F
ASTM D696
Electrical Properties Metric English Comments
Volume Resistivity 1.80e+14 ohm-cm
1.80e+14 ohm-cm
ASTM D257
Surface Resistance >= 5.60e+16 ohm
>= 5.60e+16 ohm
ASTM D257
Insulation Resistance 1.10e+13 ohm
1.10e+13 ohm
100VDC, 60 sec; Mil-I-46058C
Dielectric Constant 3.36
3.36
ASTM D150
Dielectric Strength 18.5 kV/mm
470 kV/in
ASTM D149
Dissipation Factor 0.011
0.011
ASTM D150
Descriptive Properties Value Comments
Adhesive Type 300MP
Liner 58# PCK 4.2
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved