Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polypropylene, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330 |
3M ScotchCal™ 3698E Graphic Film Material 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7880 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Material 7880 is a 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for traditional.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7924 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | to ABS, 90°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 9009 Double Coated Tapes with Adhesive 300 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Stainless Steel, 90° Peel, Initial, 20 min dwell at RT; ASTM D3330 |
3M 9017FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 9017FL and 9018FL are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. T.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.64642 kN/m | 3.6875 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |