Material Notes:
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear values even at elevated temperatures. They also offer low “outgassing” properties, which is an important consideration for the aerospace, automotive and electronic industriesInformation provided by 3M
Physical Properties Metric English Comments
Thickness 29.5 microns
1.16 mil
Mechanical Properties Metric English Comments
Peel Strength 0.1972 kN/m
1.125 pli
High Surface Energy Plastic (ABS), Ultimate bond, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
0.394 kN/m
2.25 pli
High Surface Energy Plastic (ABS), 72 hr. dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
0.526 kN/m
3.00 pli
to Stainless Steel, 20 min dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
0.93128 kN/m
5.3125 pli
to Stainless Steel, 72 hr. dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
1.3038 kN/m
7.4375 pli
to Stainless Steel, Ultimate bond, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
Thermal Properties Metric English Comments
CTE, linear 19.9 µm/m-°C

@Temperature 125 - 175 °C
11.1 µin/in-°F

@Temperature 257 - 347 °F
First heat; ASTM-D696
58.4 µm/m-°C

@Temperature 25.0 - 175 °C
32.4 µin/in-°F

@Temperature 77.0 - 347 °F
Second heat; ASTM-D696
Thermal Conductivity 0.178 W/m-K

@Temperature 51.0 °C
1.24 BTU-in/hr-ft²-°F

@Temperature 124 °F
ASTM C518
0.183 W/m-K

@Temperature 71.0 °C
1.27 BTU-in/hr-ft²-°F

@Temperature 160 °F
ASTM C518
0.187 W/m-K

@Temperature 101 °C
1.30 BTU-in/hr-ft²-°F

@Temperature 214 °F
ASTM C518
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+15 ohm-cm
4.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Insulation Resistance >= 9.40e+10 ohm
>= 9.40e+10 ohm
Cycle #410, test voltage = 100 VDC, MIL-I-46058C
>= 1.50e+11 ohm
>= 1.50e+11 ohm
Cycle #4, test voltage = 100 VDC, MIL-I-46058C
>= 9.70e+12 ohm
>= 9.70e+12 ohm
24 hr after moisture resistance
>= 1.00e+15 ohm
>= 1.00e+15 ohm
Before moisture resistance, test voltage = 100 VDC, MIL-I-46058C
Dielectric Constant 2.92

@Frequency 1000 Hz
2.92

@Frequency 1000 Hz
ASTM D-150-92
Dielectric Strength 43.3 kV/mm
1100 kV/in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
Dissipation Factor 0.0025

@Frequency 1000 Hz
0.0025

@Frequency 1000 Hz
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Liner 55# Densified Kraft - 3.2 mils thick with printed liner