Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | IPC-TM-650.2.5.6.2 |
Park Electrochemical Nelco® N4000-29 BC® Buried Capacitance™ Multifunctional Epoxy The Nelco N4000-29 is a lead-free, low-CTE, high Tg multifunctional epoxy substrate which has been designed for use in standard multilayer PWB designs and today’s toughest, high-performance, lead-f.. |
|||
Dielectric Strength | 43.3 - 51.2 kV/mm | 1100 - 1300 kV/in | ASTM D149 |
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Dielectric Strength | 43.5 kV/mm | 1100 kV/in | |
Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 60 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....)ISO data provided .. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | ASTM D149 |
Arlon 10502R020 0.020" (0.508 mm) Cured Silicone Rubber (Unsupported) Design/Construction:Material: Cured Silicone RubberLiner: Polyethylene Recommended Cure Cycle: Product delivered curedRecommended Post Cure Cycle: Product delivered post-curedAppearance: Red silicon.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | 500 vac, rms. [60 Hz]/sec; ASTM D149-92 |
3M 941 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | 500 vac, rms. [60 Hz]/sec; ASTM D149-92 |
3M 9461P Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | 500 vac, rms. [60 Hz]/sec; ASTM D149-92 |
3M 9461PC Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | 500 vac, rms. [60 Hz]/sec; ASTM D149-92 |
3M 965 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | 500 vac, rms. [60 Hz]/sec; ASTM D149-92 |
3M 966 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | IPC TM-650 2.5.6.2 |
Arlon CLTE Microwave Printed Circuit Board Substrate CLTE is a ceramic powder-filled and woven micro fiberglass reinforced PTFE composite engineered to produce a stable, low water absorption laminate with a nominal Dielectric Constant of 2.98.Ceramic/.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | ASTM D149 |
Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Appearance: Blue silicone gumThis data represents typical values for the production material. The d.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | 12 to 15 mil coating; ASTM D149 |
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 5388 is a one-part, blue pigmented, rapid heat curing powder resin, designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a var.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | ASTM D257 |
3M Scotch-Weld™ DP-100NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP-100NS is a two-part adhesives offering fast cure and machinability.Information provided by 3M |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | ASTM D149 |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Dielectric Strength | 43.3 - 51.2 kV/mm | 1100 - 1300 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | 500 vac, rms. [60 Hz]/sec; ASTM D149-92 |
3M 9462P Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | |
Aremco Aremco-Bond™ 2320 High Performance Epoxide Toughened, Unfilled, Fast-Setting, BPA Free, 2:1, High Peel & Shear Strength |
|||
Dielectric Strength | 43.3 kV/mm | 1100 kV/in | IPC-TM-650.2.5.6.2 |
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW.. |
|||
Dielectric Strength | 43.3 - 51.2 kV/mm | 1100 - 1300 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |