Material Notes:
3M™ Adhesive Remover is ideal for the removal of adhesive residue or for surface preparation prior to use of adhesive and can be used for cleaning heavy oils, greases, silicone, tar and paraffinic materials such as Cosmoline™ and wax.Information provided by 3M
Physical Properties Metric English Comments
Density 0.793 g/cc
0.0286 lb/in³
Aerosol
0.840 g/cc
0.0303 lb/in³
Bulk
Viscosity 0.80 cP
0.80 cP
Bulk
>= 100 cP
>= 100 cP
Aerosol
Thermal Properties Metric English Comments
Boiling Point 171 - 189 °C
340 - 372 °F
Bulk
Flash Point -46.0 °C
-50.8 °F
Aerosol
47.0 °C
117 °F
Bulk
Descriptive Properties Value Comments
Appearance Colorless to light yellow
Bulk
Transparent
Aerosol
Base Citrus Extra