Polymer Property : Boiling Point = 340 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 171 - 189 °C
340 - 372 °F
Bulk
3M Adhesive Remover
3M™ Adhesive Remover is ideal for the removal of adhesive residue or for surface preparation prior to use of adhesive and can be used for cleaning heavy oils, greases, silicone, tar and paraffinic ..
Boiling Point 171 °C
340 °F
Blue River Coatings Hyfro-Flex II PIR (Heat Reflective) Polyurethane Top Coat
BLUE RIVER COATINGS HYDRO-FLEX II PIR POLYURETHANE TOPCOAT is a high performance, heat reflective, single component water dispersible polyurethane. HYDRO-FLEX II PIR is formulated with heat reflecti..
Boiling Point 171 °C
340 °F
Blue River Coatings Hyfro-Flex Polyurethane Top Coat
BLUE RIVER COATINGS HYDRO-FLEX POLYURETHANE TOPCOAT is a water dispersible polyurethane. When the customer receives HYDRO-FLEX, it is already formed in the container, where as the solvent base type,..
Boiling Point 171 °C
340 °F
Blue River Coatings Hydro-Gloss 2-Part Polyurethane Top Coat
BLUE RIVER COATINGS HYDRO-GLOSS 2-PART POLYURETHANE TOPCOAT is a water dispersible polyisocyanate coating. HYDRO-GLOSS provides outstanding coverage, excellent durability, and ease of application as..