3M Balsa Panels

Category Wood and Natural Products , Wood
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Balsa Panels.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Balsa Panels are made of end grain balsa, a highly processed ultra light wood product, imparts impressive strength and stiffness to the sandwich panel. The end grain confiation of balsa provides high resistance to crushing and is very difficult to tear apart. End grain balsa cored panels also have the ability to handle excessive dynamic loads with high resistance to fatigue. The balsa panels end grain orientation gives it exceptional compression and shear properties. As an added benefit, panels providing good thermal and acoustic insulation. Balsa panels are available in 9.5 lb/ft3 density.Information provided by 3M
Physical Properties Metric English Comments
Density 0.128 - 0.176 g/cc
0.00462 - 0.00636 lb/in³
Mechanical Properties Metric English Comments
Compressive Strength 13.07 MPa
1895 psi
ASTM C365
Compressive Modulus 4.07 GPa
590 ksi
ASTM C365
Shear Modulus 0.159 GPa
23.1 ksi
ASTM C273
Shear Strength 2.98 MPa
432 psi
ASTM C273
Processing Properties Metric English Comments
Moisture Content 9.66 %
9.66 %