3M Dyneon™ CC607 Custom Fluoropolymer Compound  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ CC607 Custom Fluoropolymer Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound consists of a mixture of 35% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.23 g/cc
2.23 g/cc
ASTM D4745
Bulk Density 0.760 g/cc
0.0275 lb/in³
ASTM D4745
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.1 MPa
1900 psi
ASTM D4745
Elongation at Break 180 %
180 %
ASTM D4645