3M Dyneon™ Dynamar™ FX 9614 Polymer Processing Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoset , Fluoropolymer, TS
Manufacturer 3M Dyneon™
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ Dynamar™ FX 9614 Polymer Processing Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dynamar polymer processing additive FX 9614 is a free flowing granular concentrate form of a fluoropolymer designed for use at very low levels to improve the processing of thermoplastics. At the very low levels (typically 50-800 ppm) necessary to improve processing, it does not alter or detract from the good mechanical properties associated with high strength plasticsFeature and BenefitsBroadens extrusion processing capabilities of polyolefin resinsIdeal for use in low melt index LLDPE and high molecular weight HDPE resinsExcellent thermal stability for high temperature processingReduces or eliminates melt fractureReduces or eliminates die build-upLowers apparent melt viscosityFor use at very low levelsFree-flowing fluoropolymer-based processing aidCan offer performance and cost advantagesInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Bulk Density 0.700 g/cc
0.0253 lb/in³
Particle Mesh Size <= 10 Mesh
<= 10 Mesh
Descriptive Properties Value Comments
Color Off-white
Form Granular
Inorganic Additives % 10