Material Notes:
3M™ Dyneon™ Fluoroplastic Agglomerate ET 6210AZ is a melt processable fluoroplastic consisting mainly of alternating tetrafluoroethylene and ethylene monomer units (ETFE). This partially crystalline fluorothermoplastic offers a valuable combination of properties. This agglomerate form can also be used for compounding.Features and Benefits:Wide service temperature range –200° to +150°CLow flammabilityExcellent electrical and mechanical propertiesVery good resistance to solvents and chemicalsHigh resistance to outdoor weatheringHigh light transmission in the visible and UV rangesNon-stick characteristicsExcellent tear resistanceLow permeabilityGood resistance to radiationInformation provided by the Dyneon division of 3M.
Physical Properties Metric English Comments
Specific Gravity 1.73 g/cc
1.73 g/cc
ASTM D792
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 297 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 567 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 267 °C
513 °F
ASTM D4591
Maximum Service Temperature, Air 150 °C
302 °F
DIN 57207 part 6
Minimum Service Temperature, Air -200 °C
-328 °F
Oxygen Index >= 30 %
>= 30 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 2.58

@Frequency 1.00e+6 Hz
2.58

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 140 kV/mm

@Thickness 0.100 mm
3560 kV/in

@Thickness 0.00394 in
ASTM D149
Users viewing this material also viewed the following: