Polymer Property : Melting Point = 267 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 267 - 299 °C
513 - 570 °F
Indium Corp. Indalloy® 228 Pb-Sn-Ag Solder Alloy
(Sn10) High temp solder. Not recommended for applications above 120°C, due to formation of eutectic.Information provided by the manufacturer, Indium Corporation.
Melting Point 267 °C
513 °F
ASTM D3418
Samyang Tramid® 210P Polyamide, High Productivity
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210P is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT..
Melting Point <= 267 °C
<= 513 °F
Peak Melting Point; ExxonMobil method
ExxonMobil HDPE HD 6719.17 High Density Polyethylene Copolymer Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
Melting Point <= 267 °C
<= 513 °F
Peak Melting Point; ExxonMobil method
ExxonMobil HDPE HD 6719.62 High Density Polyethylene Copolymer Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
Melting Point 267 °C
513 °F
DAM; 10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Zytel® FR95G25V0NH NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 ZYTEL FR95G25V0NH NC010 is 25% glass fiber reinforced flame retardant polyamide halogen and red phosphorous free with high flow and excellent long t..
Melting Point 267 °C
513 °F
ASTM D4591
3M Dyneon™ ET 6235Z Fluorothermoplastic Granules
ET 6235 is a melt-processable fluoroplastic consisting mainly of alternating tetrafluoroethylene and ethylene monomer units (ETFE). Applications: Its excellent properties make Dyneon ET 6235Z ideal ..
Melting Point 267 °C
513 °F
ASTM D4591
3M Dyneon™ ET 6210AZ Fluoroplastic Agglomerate
3M™ Dyneon™ Fluoroplastic Agglomerate ET 6210AZ is a melt processable fluoroplastic consisting mainly of alternating tetrafluoroethylene and ethylene monomer units (ETFE). This partially crystalli..