Material Notes:
3M™ Dyneon™ Fluoroelastomer FC 2145 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FC 2145 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stabilityComposition: di-polymer of vinylidene fluoride and hexafluoropropyleneLow viscosity gumstock without incorporated curativesProcess targets: injection and transfer molding, extrusion, calendering and coatingsFC 2145 is amine or bisphenol curableInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Mooney Viscosity 28

@Temperature 121 °C
28

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 12.17 MPa
1765 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 184 %
184 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D4645
100% Modulus 0.00555 GPa
0.805 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 16 %
16 %
Aged 70 hours @ 200°C, Method B, -214 O-rings; ASTM D395
Thermal Properties Metric English Comments
Transformation Temperature -18.0 °C
-0.400 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 65.9 %
65.9 %
Descriptive Properties Value Comments
Color Straw
MH, Maximum Torque 18.9 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque 0.8 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
Solubility Ketones and Esters
t`50, Time to 50% cure 2.4 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure 3.5 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min 1.9 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C