Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
Specific Gravity | 1.80 - 1.95 g/cc | 1.80 - 1.95 g/cc | |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
Specific Gravity | 1.80 - 1.95 g/cc | 1.80 - 1.95 g/cc | |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
NextGen Adhesives P907-30 Optical Assembly Adhesive Description: NGAC P907-30 is a high viscosity, controlled flow encapsulant designed for microelectronics applications requiring low shrinkage and high reliability performance.Advantages and Applicat.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
Parker Chomerics CHO-SHIELD® 576 Platable Silver Epoxy Coating Description: CHO-SHIELD® 576 coating is a two component, silver filled, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric plastic substrate. This coating .. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
Parker Chomerics CHO-SHIELD® 611 Part A Conductive Coating Comments: Variant of CHO-SHIELD 596Typical Applications:Protecting EMI flangesInformation provided by Chomerics |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D792 |
Custom Resins Vexel™ E20GF45 FR , 45% Glass Reinforced, Flame Retardant PET
(discontinued **) Description: Vexel™ E20GF45 FR is a 45% glass fiber reinforced, flame retardant PET. Information provided by Custom Resins. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ASTM D792 |
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ASTM D792 |
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc @Thickness 1.57 mm |
1.80 - 1.90 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP509 Glass Fabric Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc @Thickness 1.57 mm |
1.80 - 1.90 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP511 Glass Fabric Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D297, 15 |
Seals Eastern 7265 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Vito.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2FL24 ETFE LNP* THERMOCOMP* 2FL24 is a compound based on ETFE resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is Wear Resistant. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | Cured |
Tra-Con Tra-Bond 526W01 Microelectronics Grade Encapsulant TRA-BOND 526W01 is a one component micro-electronics grade controlled flow encapsulant designed to protect wire bonds and bare die. TRA-BOND 526W01 has a low coefficient of thermal expansion and low.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | at 25°C |
Daikin DAI-EL LT-302 Fluoroelastomer, Low Temperature Grade, 64% Fluorine Content Features: Flexible up to -30°C, excellent low temperature sealing.Information provided by Daikin Industries. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ASTM D792-66 |
BCC Products Kwik Kast BC 8645 Urethane Casting BCC Kwik Kast/Gray is a two component, fast setting polyurethane reproduction plastic. BC8645 has been reformulated to enhance filler suspension and avoid hard packing @ 77ºF. Uses include; tracing.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ASTM D792-66 |
BCC Products SLO-KAST BC 8009 Urethane Casting Slo-Kast is a low viscosity, medium setting, easy to use casting material. This polyurethane system features extremely low shrinkage when properly cured. Unlike Kwik-Kast, BC 8009 offers the user lo.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2145 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2145 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2176 Fluoroelastomer Composition: di-polymer of vinylidene fluoride and hexafluoropropyleneAbility for fast cure cycles with excellent processing safetyMedium viscosityProcess targets: compression and transfer molding, .. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2261Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2261Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FE 5620Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5620Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FE 5642 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5642 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FG 5630Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FG 5630Q can be compounded using standard water cooled internal mixers or two-roll mills. The “dry” ingredients should be blended before adding to the masticated gum... |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | |
Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical app.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | |
BCC Products Kwik Kast BC 8001 Urethane Casting BC8001 is an advanced fast cast polyurethane tooling system. It features low viscosity, low exotherm and minimal shrinkage. It cures hard, yet more durable resulting in less brittle parts. Designed.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2120 Fluoroelastomer 3M™ Dyneon™ Flouroelastomer FC 2120 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D395 |
Parker Chomerics CHOFORM® 5560 Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |