3M™ Dyneon™ Fluoroelastomer FG 5661 can be compounded using standard water cooled internal mixers or two-roll mills. The “dry” ingredients should be blended before adding to the masticated gum. For best results, FG 5661 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks display excellent processing characteristics and storage stability.Composition: Di-polymer of vinylidene fluoride and hexafluoropropyleneHigh mooney version of FG 5630QIn compliance with US FDA 21 CFR 177.2600When compared to diamine cured compounds this product gives excellent mold release, better mold flow, superior compression set resistance, and superior water resistance at elevated temperaturesProprietary incorporated cure technologyInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Mooney Viscosity 60

@Temperature 121 °C
60

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 15.33 MPa
2223 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 193 %
193 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.006950 GPa
1.008 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 14 %
14 %
Aged 70 hours @ 200°C, Method B, O-rings -214; ASTM D395
Thermal Properties Metric English Comments
Transformation Temperature -18.0 °C
-0.400 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 65.9 %
65.9 %
Descriptive Properties Value Comments
Color Opaque Off-White
MH, Maximum Torque 22.3 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque 2.4 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
Mooney Scorch, MS >50
@ 121°C
1
Point rise at 25 min @ 121°C
Solubility Ketones and Esters
t`50, Time to 50% cure 1.9 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure 2.6 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min 1.4 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C