3M Dyneon™ Fluorel™ FLS-2650 Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ Fluorel™ FLS-2650 Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 70.3%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 1.8% Luperco™ 101XL Peroxide, and 2.5 % Triallyl Isocyanurate (TAIC). Peroxide curable high fluorine gum with low swell in aggressive fluids. Used in Peroxide Cure Grades.
Physical Properties Metric English Comments
Density 1.89 g/cc
0.0683 lb/in³
Mooney Viscosity 50

@Temperature 121 °C
50

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Tensile Strength, Ultimate 18.0 MPa
2610 psi
Tensile Strength, Yield 5.40 MPa
783 psi
M100
Elongation at Break 230 %
230 %
Coefficient of Friction, Dynamic 0.80
0.80
Compression Set 28 %

@Temperature 200 °C
28 %

@Temperature 392 °F
70 hr; ASTM D395B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -7.00 °C
19.4 °F
TR10