Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ PFA 6505N Perfluoroalkoxy Fluorothermoplastic  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ PFA 6505N Perfluoroalkoxy Fluorothermoplastic  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight grade (lowest MFI) offers maximum stress crack resistance and tensile strength. It is ideal for applications such as tubing and sheeting. Dyneon™ PFA 6515 and PFA 6525N are designed for higher speed or higher shear processing such as injection molding and wire insulation. Dyneon PFA 6500 series products achieve the excellent property balance for which PFA is known including wide service temperature range (-200° to +260°C), almost universal chemical and solvent resistance, outstanding mechanical properties, resistance to weathering, low friction/non-stick behavior, high dielectric strength, and flame resistance.Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D792
Melt Index of Compound 5.0 g/10 min

@Load 5.00 kg,
Temperature 372 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength at Break 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 410 %
410 %
ASTM D638
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 308 °C
586 °F
ASTM D4591
Flammability, UL94 V-0
V-0
Oxygen Index >= 95 %
>= 95 %
ASTM D2863