3M™ Dyneon™ PFA 6910GZ is a 50% solids fluorothermoplastic aqueous dispersion. It is a copolymer of tetrafluoroethylene and perfluorinated comonomers, with a melt viscosity several orders of magnitude lower than PTFE. It can be utilized in coating system formulations and in combination with PTFE dispersions, binding resins and pigments. Due to its small particle size, Dyneon PFA 6910GZ can be utilized for sealing extremely fine-pored substrates.Features and Benefits:Very fine particle sizeGood thermoplastic machinabilityOutstanding soil and dirt repellencyExcellent UV stabilityInformation provided by the Dyneon division of 3M.
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
Dry Polymer; ASTM D792
Bulk Density 1.10 g/cc
0.0397 lb/in³
Dispersion; ASTM D1298
Solids Content 22 %
22 %
ASTM D4441
Particle Size 90 µm
90 µm
ISO 13321
pH 9.0
9.0
ASTM E70
Viscosity Measurement 9.0
9.0
[mPa], D=30<sup>-1</sup>; DIN 54 453
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 372 °C
15 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Storage Temperature 5.00 - 30.0 °C
41.0 - 86.0 °F
No freezing
Thermal Properties Metric English Comments
Melting Point 306 °C
583 °F
ASTM D4591
Descriptive Properties Value Comments
Surface Active Ingredients non-ionic