Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond CSA-NF Cyanoacrylate Surface Activator Permabond C Surface Activator (CSA-NF) is used in conjunction with Permabond cyanoacrylate adhesives to promote a faster cure and to extend their gap-filling capabilities. It significantly reduces t.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET510 Epoxy Resin PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET536 Epoxy Resin PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bo.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET5401 Epoxy Resin PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HH120 Anaerobic Threadlocker Permabond® HH120 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Its high viscosity allows for .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HH131 High Temperature Threadlocker Permabond® HH131 is a very high temperature resistant, high strength anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. It is used for .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM128 Anaerobic Threadlocker Permabond® HM128 Threadlocker is a high strength adhesive for permanent assembly. It is typically used for preventing vibration loosening of bolts, studs and cap screws. Full cure to a cross-linked.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM165 Anaerobic Retainer Permabond® HM165 is a high viscosity anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It is best suited for cylindrical parts and where high temperatu.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LH050P Pure Anaerobic Threadsealant PERMABOND® LH050 PURE anaerobic pipe sealant is single component paste that cures only when in contact with metal parts and oxygen is excluded. The sealant fills up the entire space between male an.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond MH196 Anaerobic Gasketmaker Permabond® MH196 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA430 Acrylic Adhesive & Initiator PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA435 Toughened Acrylic Adhesive & Initiator PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA436 Toughened Acrylic Adhesive PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV625 UV-curable Adhesive PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistan.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV640 UV-curable Adhesive PERMABOND UV640 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV648 UV-curable Adhesive PERMABOND UV648 is a UV-curing adhesive developed for use on plastics. It has good adhesion to acrylic and contains a long-wavelength photo initiator to allow it to cure through UV-stabilized plasti.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV670 UV-curable Adhesive PERMABOND UV670 is a single part, fast curing, UV curable adhesive. The cured adhesive is tough, flexible and has excellent impact resistance. Permabond UV670 is well suited for bonding glass to met.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F807 Black Polyetheretherketone (PEEK) Liquid Dispersion Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HH040 Anaerobic Retainer Permabond® HH040 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure unitiz.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HH040 Pure NSF 61 Approved Anaerobic Retainer Permabond® HH040 PURE is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure u.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond MM115P Pure Anaerobic Threadlocker Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A1044 Anaerobic Threadsealant Permabond® A1044 is a rapid curing sealant designed to lock and seal metal pipe connections, offering very good resistance to even the most aggressive chemicals. Permabond A1044 can be used to seal.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond MH052 Anaerobic Threadsealant Permabond® MH052 is ideal for the sealing of threaded joints. It is approved for use with natural gas and LPG for working pressure up to 20 bar (290 psi) and also for gaseous oxygen up to 10 bar (1.. |
|||
Storage Temperature | 5.00 - 27.0 °C | 41.0 - 80.6 °F | 3 months |
ACC QSil 58 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting QSil 58 is a red, high temperature, self-leveling, two-component silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section C.. |
|||
Storage Temperature | >= 5.00 °C | >= 41.0 °F | cool dry place |
Gwent Electronic Materials R2040227D1 Hot Melt Conductive Adhesive for Diagnostic Sensors This is a one-component water based polyurethane dispersion used for bonding unsupported PVC foils. This can be used in many different diagnostic applications such as test cards, assays and support.. |
|||
Storage Temperature | 5.00 °C | 41.0 °F | |
Henkel Hysol EA 9257 Primer Waterborne, corrosion-inhibiting primer, maintains surface bondability after multiple prebonding cure cycles. Meets SCAQMD Rule 1124. Replacement for Hysol EA 9210B.Applications: Sprayable Low Visc.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A130 Anaerobic Threadlocker Designed for the locking and sealing of metal parts, Permabond® A130 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used t.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A136 Anaerobic Gasketmaker Permabond® A136 is an anaerobic material designed for making 'formed in situ' gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets thereby offering potent.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F810 Black Polyetheretherketone (PEEK) Liquid Dispersion Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, .. |