3M Dyneon™ TF 2024 PTFE Paste Extrusion Powder  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 2024 PTFE Paste Extrusion Powder  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 500. Average particle size 500µm. Used for unsintered tapes and sealing cords.Dyneon offers a family of PTFE fine powder paste extrusion resins. These products are well suited for a variety of applications, including tubing, hose, pipe liners, tapes, wire and cable, diaphragms and textile/fiber. Available grades are designed to balance process properties such as reduction ratio, and performance properties, such as tensile strength, shrinkage, flex life and permeations. Data provided by Dyneon.
Physical Properties Metric English Comments
Density 2.15 g/cc
0.0777 lb/in³
Sintered moldings; ASTM D4894/D4895
Apparent Bulk Density 0.510 g/cc
0.0184 lb/in³
DIN 53 466
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 28.0 MPa

@Thickness 1.60 mm
4060 psi

@Thickness 0.0630 in
Sintered moldings; ASTM D4894/4895
Elongation at Break 340 %
340 %
Sintered Molding; ASTM D4894
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
IEC 60093