3M Dyneon™ TF 2072 PTFE  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 2072 PTFE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Processable by standard paste extrusion methodTF 2071 and TF 2072 have a wide processing range because of high maximum allowable reduction ratioTF 2072 is recommended for thin-wall, small diameter tubing and wire and cable insulation, processed by paste extrusion method at reduction ratio up to 3000:1High reduction ratios allow more cost-effective extrusion because larger performs can be usedInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Bulk Density 0.500 g/cc
0.0181 lb/in³
ASTM D4895
Density 2.16 g/cc
0.0780 lb/in³
ASTM D4895
Particle Size 600 µm
600 µm
average; ASTM D4895
Thickness 63.0 microns
2.48 mil
ASTM D4895
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D4895
Elongation at Break 360 %
360 %
ASTM D4895
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+19 ohm-cm
1.00e+19 ohm-cm
IEC 60093
Surface Resistance 1.00e+18 ohm
1.00e+18 ohm
IEC 60093
Descriptive Properties Value Comments
Extrusion Pressure 40 MPa
reduction ratio 1600, ASTM D4894
Reduction Ratio Range 50-3000:1
Dyneon Method
Users viewing this material also viewed the following: