Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ THV 610GZ Fluoroplastic Granules

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ THV 610GZ Fluoroplastic Granules.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Dyneon™ Fluoroplastic Granules THV 610GZ provides a balance of low permeation, thermal stability, and melt processability. It can be used to prepare molded parts and extruded films, tubes, profiles and wire coatings. It is useful for applications that require flexibility and good chemical resistance. This product processes at higher temperatures than that of 3M THV grades; therefore, the use of corrosion - resistant equipment is suggested.Features and Benefits:Excellent flexibilityHigher transparencyExcellent chemical permeation resistanceBondable to itself and other substrates (for multi-layer constructions)Processing profile allows co-processing with other plastics and hydrocarbon elastomersInformation provided by the Dyneon division of 3M.
Physical Properties Metric English Comments
Specific Gravity 2.04 g/cc
2.04 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 265 °C
10 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 0.490 GPa
71.1 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 185 °C
365 °F
ASTM D4591
Users viewing this material also viewed the following: