Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.490 - 3.34 GPa | 71.1 - 485 ksi | Average value: 0.736 GPa Grade Count:15 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Modulus | 0.490 - 4.36 GPa | 71.1 - 633 ksi | Average value: 1.26 GPa Grade Count:14 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Flexural Modulus | 0.490 GPa | 71.1 ksi | ASTM D790 |
SK Chemicals SKYPEL M572CR Special Grade Copper Resistance SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Flexural Modulus | 0.490 GPa | 71.1 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.490 GPa | 71.1 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.490 GPa | 71.1 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.490 GPa | 71.1 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.490 GPa | 71.1 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.490 GPa | 71.1 ksi | ASTM D790 |
DuPont™ Surlyn® 8140 Ionomer Resin, Sodium Surlyn® 8140 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON F-104 PTFE Fine Powder Processing Methods: Paste extrusion, calendering.Applications: Unsintered tape, sealing tape, low specific gravity tape, tape for wrapping flat cables, tubes.Information provided by Daikin Industrie.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON F-201 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON F-205 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON F-302 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Small to large diameter tubes, flexible hoses, shrinkable tubes, heavy duty electric wires smaller than AGW18, and jackets.Information provided by .. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON M-12 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Useful in making products requiring fine texture, especially insulation skiving tapes. Also allows uniform mixing of inorganic fill.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Suited to molding of large billets, has nearly the same molding characteristics of M-12. Also allows uniform mixing of inorganic fi.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic or semi-automatic compression molding, isostatic molding, and ram extrusion.Features: Good fill characteristics particularly into .. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON MG-1040 PTFE 20% Glass Fiber Filled Molding Powder 20% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder 20% glass fiber and 5% graphite filled. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (e.g. piston rings, bearing pads, and packings)Inform.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON MG-1241F PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder, High Apparent Density, Free Flow 20% glass fiber and 5% graphite filled. High apparent density and free-flowing properties. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder 15% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON MG-2060 PTFE 30% Graphite Filled Molding Powder 30% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON MG-6030 PTFE 15% Carbon Fiber Filled Molding Powder 15% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by .. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON MG-6050 PTFE 25% Carbon Fiber Filled Molding Powder 25% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by .. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON MG-1030F PTFE 15% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Flexural Modulus | 0.490 - 0.588 GPa | 71.1 - 85.3 ksi | ASTM D790 |
Daikin POLYFLON MG-1050 PTFE 25% Glass Fiber Filled Molding Powder 25% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Flexural Modulus | 0.490 GPa | 71.1 ksi | ASTM D790 |
DuPont Surlyn® PC2000
(discontinued **) DuPont™ Surlyn® PC2000 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA c.. |