Material Notes:
Information provided by 3M
Physical Properties Metric English Comments
Density 3.90 g/cc
0.141 lb/in³
Permeability 13
13
[ft<sup>3</sup>/min/ft<sup>2</sup>], Air w/o sizing
Thickness 480 microns
18.9 mil
Fiber Count 3330 dtex
3000 denier
roving
Mechanical Properties Metric English Comments
Tensile Strength at Break 3100 MPa
450000 psi
filament 25.4mm
Tensile Modulus 379 GPa
55000 ksi
filament
Tear Strength 45.1 kN/m
258 pli
Fill, Breaking Strength w/o Sizing
53.0 kN/m
302 pli
Warp, Breaking Strength w/o Sizing
Thermal Properties Metric English Comments
CTE, linear 8.00 µm/m-°C

@Temperature 100 - 1100 °C
4.44 µin/in-°F

@Temperature 212 - 2010 °F
Melting Point 2000 °C
3630 °F
Optical Properties Metric English Comments
Refractive Index 1.74
1.74
Component Elements Properties Metric English Comments
Al2O3 99 %
99 %
Electrical Properties Metric English Comments
Dielectric Constant 9.0

@Frequency 9.375e+9 Hz
9.0

@Frequency 9.375e+9 Hz