Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.90 - 3.92 g/cc | 0.141 - 0.142 lb/in³ | Sintered |
Nabaltec GRANALOX® NM 9922 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 105 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 105-71 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 115-25 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 115-71 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 115P Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 313 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 315 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 615-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 615-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 625-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 625-31 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | Sintered |
Nabaltec NABALOX® NO 713-10 MF Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 713-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 713-40 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 715-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 725-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
NanoScale NanoActive® Aluminum Oxide NanoActive Al2O3 is produced using proprietary processes to obtain high specific surface area, low density, amorphous material with high adsorption capacity and chemical reactivity. NanoActive Al2O3.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 4406 PTFE, 60% Bronze Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings.Data provided by Dyneon. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
MarkeTech Repton 136 Aluminum Oxide Brand 136 features: Molding-structural.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when the.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Misumi Alumina 99 Aluminum Oxide, Al2O3 Information provided by MISUMI Corporation. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0390 BK Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Rubalit® 710 Alumina, 99.6% Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | DIN EN 623-2 |
CeramTec V 679 Alumina, 99.7% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ASTM-C 20 |
CoorsTek AD-996 99.6% Alumina |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ASTM-C 20 |
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
BASF Paliotan® Yellow L 1145 Color Additive Description: Pigment combination based on Bismuth VanadateSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, and Airdrying systems.Information provided by BASF |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
3M Nextel™ DF-11 Woven Fabric 610 Information provided by 3M |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
3M Nextel™ DF-19 Woven Fabric 610 Information provided by 3M |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-B60 PTFE Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |