3M Polystyrene Foam Insulation 78 Spray Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Polystyrene Foam Insulation
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Polystyrene Foam Insulation 78 Spray Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high strength, industrial grade spray adhesive that is typically used for bonding most types of insulation such as fiberglass, expanded polystyrene foam, and extruded polystyrene foam.Features:Aggressively tacky industrial grade spray adhesive that is typically used for bonding most types of insulation such as fiberglass, expanded polystyrene foam, and extruded polystyrene foam.Will not dissolve polystyrene foamHigh coverage productCapable of both one a two surface bondingInformation provided by 3M
Physical Properties Metric English Comments
Density 0.755 g/cc
0.0273 lb/in³
Aerosol
0.791 g/cc
0.0286 lb/in³
Bulk
Solids Content 19.1 %
19.1 %
Aerosol
35 %
35 %
Bulk
Volatile Organic Compounds (VOC) Content 508 g/l
508 g/l
Viscosity <= 500 cP
<= 500 cP
Bulk
Descriptive Properties Value Comments
Appearance Translucent
Aerosol
Translucent
Bulk
Base Synthetic Elastomer
Aerosol
Synthetic Elastomer
Bulk