Material Notes:
3M™ Cold Shrink Quick Splice Low Voltage QSLV-M are open-ended tubular rubber sleeves with sealing mastic on each end which are factory expanded and assembled onto a unique three-core system. Two cores, one on each end, are removed after the QSLV-M insulator has been centered over an inline connector, allowing the ends of the tube to shrink and form a water-resistant seal. The third, center segment of the core remains inside the cold shrink tube, acting as a support structure. Sizing of the cores and tube, along with the sealing mastic on each end, is designed to accommodate the variance in connectors and connector crimping techniques and final dimensions without degrading the seal and insulating characteristics of the EPDM rubber tube, while making core removal easy. Two diameter sizes will cover a range of 1000 volt or less cable from 8 AWG through 500 kcmil, copper and aluminum conductors with crimped connectors.Information provided by 3M
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.65 MPa
1400 psi
ASTM D412-75
Elongation at Break 750 %
750 %
ASTM D412-75
300% Modulus 0.00331 GPa
0.480 ksi
ASTM D412-75
Tear Strength 25.8 kN/m
147 pli
Die C; ASTM D624C-73
Electrical Properties Metric English Comments
Dielectric Strength 11.1 kV/mm
282 kV/in
7 days @ 90°C in water; ASTM D149-75
14.4 kV/mm
365 kV/in
Original; ASTM D149-75
Processing Properties Metric English Comments
Moisture Content 1.8 %
1.8 %
7 days @ 90°C in water
Descriptive Properties Value Comments
Appearance Black