Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | |
Sylvin Technologies 9925-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | |
Sylvin Technologies 9960-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | |
Dow Corning SILASTIC® LS-2380 FLUOROSILICONE RUBBER 70 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D638 |
Colorite Polymers 6034 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M QI-18/57-325 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M QI-5/16-220 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Tensile Strength, Ultimate | 9.65 - 12.41 MPa | 1400 - 1800 psi | ASTM D412 |
BASF Master Builders Solutions ChemRex® CX-941 Polyurethane Adhesive CX-941 is a one-component polyurethane-based trowelable-grade structural adhesive. Its patented formula is VOC compliant and contains no chlorinated solvents or water. CX-941 provides excellent in.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M SJ-3A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412 |
3M 5300 Motor Lead Splicing Kits 3M Motor Lead Splicing Kits 5300 Series are a series of kits designed for splicing motor lead cables to incoming feeder cables. The kits accommodate the follow splice confiations:Pigtails (stub) con.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8424-8 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8426-11 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8427-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8427-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8428-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8428-18 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8429-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8429-18 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8429-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8430-9 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8454 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8459 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8460 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8462 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M QI-10/37-270 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412 |
Colorite Polymers Weatherflex™ CS7524WX (NTL01P) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8427-16 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M 8429-9 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M EC-2 Cold Shrink End Caps 3M Cold Shrink End Caps are close-ended, tubular rubber sleeves that are factory expanded and loaded onto a removable core. When positioned over the end of a cable, or other cylindrical object the c.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M EC-3 Cold Shrink End Caps 3M Cold Shrink End Caps are close-ended, tubular rubber sleeves that are factory expanded and loaded onto a removable core. When positioned over the end of a cable, or other cylindrical object the c.. |
|||
Tensile Strength, Ultimate | 9.65 MPa | 1400 psi | ASTM D412-75 |
3M EC-4 Cold Shrink End Caps 3M Cold Shrink End Caps are close-ended, tubular rubber sleeves that are factory expanded and loaded onto a removable core. When positioned over the end of a cable, or other cylindrical object the c.. |