3M R3177 Repulpable Single-Coated Tapes

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M R3177 Repulpable Single-Coated Tapes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ PTFE Glass Cloth Tape R3177 is a single-sided paper tapes coated with a patented, high tack transparent repulpable adhesive on one side and an easy release coating on the backside for smooth unwind.Information provided by 3M
Physical Properties Metric English Comments
Thickness 178 microns
7.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 9.0 %
9.0 %
Film Elongation at Yield, MD 8.0 %
8.0 %
Film Tensile Strength at Break, MD 4.59 MPa
666 psi
Film Tensile Strength at Break, TD 2.73 MPa
396 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Descriptive Properties Value Comments
Appearance White, Blue, Kraft, Red