3M Scotch® 215 Fine Line Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 215 Fine Line Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Fine Line Tape 215 is a very conformable film backed tape used to achieve excellent color separation on highly contoured surfaces.Information provided by 3M
Physical Properties Metric English Comments
Thickness 122 microns
4.80 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.9 MPa
3180 psi
ASTM D3756
Elongation at Break 1150 %
1150 %
ASTM D3756
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 212 °C
414 °F
for 30 mins removes cleanly
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Blue