Polymer Property : Tensile Strength at Break = 3180 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.9 MPa
3180 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R5185A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 21.9 MPa
3180 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Tensile Strength at Break 21.9 MPa

@Treatment Temp. 145 °C,
Time 2100 sec
3180 psi

@Treatment Temp. 293 °F,
Time 0.583 hour
Cure; ASTM D412
Styron Sprintan® SLR 4601 Solution Styrene Butadiene Rubber (S-SBR)
Composition: SPRINTAN® SLR-4601 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. The product has a medium styrene/high vinyl micro structure a..
Tensile Strength at Break 21.9 MPa
3180 psi
ASTM D3756
3M Scotch® 215 Fine Line Tape
Scotch® Fine Line Tape 215 is a very conformable film backed tape used to achieve excellent color separation on highly contoured surfaces.Information provided by 3M