3M Scotch Pad™ 819 Filament Tape Pads

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch Pad™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch Pad™ 819 Filament Tape Pads.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ ScotchPad™ Filament Tape Pad 819 is a pre-cut pad formed with layered high performance filament tape sheets featuring biaxially oriented polypropylene backing with continuous glass yarns that reinforce each sheet in both longitudinal and transverse directions. The adhesive on each sheet is specifically formulated to provide good adhesion to a wide variety of surfaces including metal, plastics, and fiberboard. Each piece of tape is coupled with a tab for easy handling and dispensing without the need for a dispenser. These sheets can be used for attaching, hinging, fastening, and sealing in many industrial, manufacturing and packaging applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 145 microns
5.70 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.6 MPa
2690 psi
ASTM D3759
Elongation at Break 6.0 %
6.0 %
ASTM D3759
Peel Strength 1.10 kN/m
6.25 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive synthetic rubber resin
Appearance Clear