Mechanical Properties Metric English Comments
Peel Strength 1.10 kN/m
6.30 pli
Copper; IPC-TM-650 2.4.8
Rogers Corporation XT/duroid™ 8100 0.004" Woven Glass Reinforced Thermoplastic Circuit Material
XT/duroid™ 8100 woven glass reinforced thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 81..
Peel Strength 1.10 kN/m
6.30 pli
To Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
Arlon 35N Fast Cure Polyimide Laminate and Prepreg
High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi..
Peel Strength 1.10 kN/m
6.30 pli
To Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
Arlon 35N Fast Cure Polyimide Laminate and Prepreg
High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi..
Peel Strength 1.10 kN/m
6.25 pli
Adhesion to Steel; ASTM D3330
3M Scotch® 8959 Bi-Directional Filament Tape
Scotch® Filament Tape 8959 is a bi-directional specialty packaging tape reinforced with continuous glass yarns in both the longitudinal and transverse direction along with a biaxially oriented poly..
Peel Strength 1.10 kN/m
6.25 pli
Stainless Steel, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
3M 8153LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..
Peel Strength 1.10 kN/m
6.25 pli
Stainless Steel, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
3M 93015LE High Strength Double Coated Tape with Adhesive 300LSE
3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl..
Peel Strength 1.10 kN/m
6.25 pli
Stainless Steel, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS..
Peel Strength 1.10 kN/m
6.25 pli
Stainless Steel, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
3M 9453LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..
Peel Strength 1.10 kN/m
6.25 pli
Polycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
3M 9579 Double Coated Tape with Adhesive 760
3M™ Double Coated Tape 9579 with 3M™ Adhesive 760 is a high-tack, hand-tearable, double coated film tape with a pressure sensitive adhesive on each side of the carrier. The medium firm adhesive fe..
Peel Strength 1.10 kN/m
6.25 pli
Stainless Steel, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Peel Strength 1.10 kN/m
6.25 pli
Stainless Steel 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Peel Strength 1.10 kN/m
6.25 pli
Adhesion to Steel; ASTM D3330
3M Scotch Pad™ 819 Filament Tape Pads
3M™ ScotchPad™ Filament Tape Pad 819 is a pre-cut pad formed with layered high performance filament tape sheets featuring biaxially oriented polypropylene backing with continuous glass yarns that ..
Peel Strength 1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330
3M 9626 Adhesive Transfer Tape with Quick Bonding Adhesive 360
3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated pai..
Peel Strength 1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Backside; ASTM D3330
3M 9626 Adhesive Transfer Tape with Quick Bonding Adhesive 360
3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated pai..
Peel Strength 1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330
3M 9626 Adhesive Transfer Tape with Quick Bonding Adhesive 360
3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated pai..
Peel Strength 1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Backside; ASTM D3330
3M 9626 Adhesive Transfer Tape with Quick Bonding Adhesive 360
3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated pai..
Peel Strength 1.10 kN/m
6.25 pli
Stainless Steel, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
3M 9628B Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Peel Strength 1.10 kN/m
6.25 pli
Stainless Steel 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
3M 9628B Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Peel Strength 1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330
3M 9629B Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Peel Strength 1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Backside; ASTM D3330
3M 9629B Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Peel Strength 1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330
3M 9629FL Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Peel Strength 1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Backside; ASTM D3330
3M 9629FL Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Peel Strength 1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Peel Strength 1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Backside; ASTM D3330
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Peel Strength 1.10 kN/m
6.25 pli
Stainless Steel, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
3M 9653LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..