3M Scotch-Weld™ 3750LM Low Melt Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 3750LM Low Melt Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent "hot tack", fast setting for corrugated, beadboard, repack, recoup and Economical, general purpose and Use with AE II LET applicator onlyInformation provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 4000 cP

@Temperature 121 °C
4000 cP

@Temperature 250 °F
Mechanical Properties Metric English Comments
Shear Strength 3.28 MPa
475 psi
On Douglas Fir
Peel Strength 1.05 kN/m
6.00 pli
on canvas
Thermal Properties Metric English Comments
Ring & Ball Softening Point 95.0 °C
203 °F
ASTM E28-99