3M Scotch-Weld™ 3792LM Low Melt Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 3792LM Low Melt Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clear multi-purpose for wood, coated paper, polyolefins and other heat-sensitive materials; P.O.P. displays and use with low melt applicator onlyInformation provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 10500 cP

@Temperature 121 °C
10500 cP

@Temperature 250 °F
Mechanical Properties Metric English Comments
Shear Strength 2.41 MPa
350 psi
On Douglas Fir
Peel Strength 2.28 kN/m
13.0 pli
on canvas
Thermal Properties Metric English Comments
Flammability, UL94 V-2
V-2
Ring & Ball Softening Point 81.0 °C
178 °F
ASTM E28-99