Mechanical Properties Metric English Comments
Shear Strength 2.41 MPa
350 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 1/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 2.41 MPa
>= 350 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® CR III 1/8-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 2.41 MPa
350 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 3/8-5052-.005 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 2.41 MPa
>= 350 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® CR-PAA™ 1/8-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 2.41 MPa
350 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.005 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength >= 2.41 MPa
>= 350 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRP - 3/8 - 8.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength >= 2.41 MPa
>= 350 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRP/OX - 1/4 - 7.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 2.41 MPa
350 psi
cured 14 days @ 50% RH; AMS3265
3M AC-730 Class C-4 (168) Aerospace Sealant
3M Aerospace Sealant AC-730 Class C are two-part, manganese-cured, non-chromate corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on a..
Shear Strength 2.41 MPa
350 psi
Lap; ASTM D1002
Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Dow Corning S2260This data represents typical values for the pr..
Shear Strength 2.41 MPa
350 psi
On Douglas Fir
3M Scotch-Weld™ 3792LM Low Melt Adhesive
Clear multi-purpose for wood, coated paper, polyolefins and other heat-sensitive materials; P.O.P. displays and use with low melt applicator onlyInformation provided by 3M
Shear Strength 2.41 MPa
350 psi
On Douglas Fir
3M Scotch-Weld™ 3797 Hot Melt Adhesive
High ball and ring; Low viscosity and Good for electrical pottingInformation provided by 3M
Shear Strength 2.41 MPa
350 psi
Overlap, Isopropyl Alcohol Wipe surface prep, FRP
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 2.41 MPa
350 psi
Overlap, Isopropyl Alcohol Wipe surface prep, Phenolic
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 2.41 MPa
350 psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, PVC
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 2.41 MPa
350 psi
Overlap, ABS
3M Scotch-Weld™ DP405 LH Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel..
Shear Strength 2.41 MPa
350 psi
Overlap, Particleboard, Substrate Failure
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 2.41 MPa
350 psi
Overlap, Melamine, Substrate Failure
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 2.41 MPa
350 psi
cured 14 days @ 50% RH; AMS3265
3M AC-730 Class C-8 (24) Aerospace Sealant
3M Aerospace Sealant AC-730 Class C are two-part, manganese-cured, non-chromate corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on a..
Shear Strength 2.41 MPa
350 psi
Overlap, Acrylic
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M
Shear Strength 2.41 MPa
350 psi
Dow Corning 3-0115 AUTOMOTIVE SEALANT
One-part, self-priming, noncorrosive, alkoxy-cure, RTV silicone rubber designed for automotive powertrain sealing applicationsInformation provided by Dow Corning