Material Notes:
3M™ Scotch-Weld™ Epoxy Adhesive DP-100 is a two-part adhesives offering fast cure and machinability.Information provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 8000 - 15000 cP
8000 - 15000 cP
Base, RVF #6 spindle, 20 rpm @ 27°C
9000 - 16000 cP
9000 - 16000 cP
Accelerator, RVF #6 spindle, 20 rpm @ 27°C
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 85
80 - 85
ASTM D2240
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature -40.0 - 20.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 68.0 °F
209 µm/m-°C

@Temperature 60.0 - 120 °C
116 µin/in-°F

@Temperature 140 - 248 °F
Thermal Conductivity 0.184 W/m-K

@Temperature 45.0 °C
1.28 BTU-in/hr-ft²-°F

@Temperature 113 °F
Glass Transition Temp, Tg 33.0 °C
91.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 3.50e+12 ohm-cm
3.50e+12 ohm-cm
ASTM D257
Dielectric Strength 33.9 kV/mm
860 kV/in
ASTM D257
Processing Properties Metric English Comments
Cure Time 1440 - 2880 min
24.0 - 48.0 hour
Descriptive Properties Value Comments
Appearance Clear/Light Amber
Users viewing this material also viewed the following: