Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotch-Weld™ DP-605NS Off-White Adhesive in Duo-Pak Cartridges  (discontinued **)

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ DP-605NS Off-White Adhesive in Duo-Pak Cartridges  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features include fast cure adhesive, semi-rigid urethane, 15-20 minutes handling strength, and excellent gap filler and non sag product for wood and plastic. Mix ratio by volume 1:1. Average T-Peel at 75°F (24°C) is 15 PIW; 180° peel tested on 0.030 inch aluminum per ASTM D 1876-61T.General info on Scotch-Weld™ Duo-Pak cartridges: Two-part room-temperature curing epoxy, urethane and acrylic adhesives especially formulated and packaged for use in the EPX Applicator.Information provided by 3M Adhesives Division.
Physical Properties Metric English Comments
Brookfield Viscosity 150000 cP

@Temperature 23.9 °C
150000 cP

@Temperature 75.0 °F
Mechanical Properties Metric English Comments
Shear Strength 0.690 MPa

@Temperature 121 °C
100 psi

@Temperature 250 °F
ASTM D1002-64
2.20 MPa

@Temperature 82.0 °C
319 psi

@Temperature 180 °F
ASTM D1002-64
6.90 MPa

@Temperature -55.0 °C
1000 psi

@Temperature -67.0 °F
ASTM D1002-64
8.60 MPa

@Temperature 24.0 °C
1250 psi

@Temperature 75.2 °F
ASTM D1002-64
Processing Properties Metric English Comments
Processing Temperature 20.0 °C
68.0 °F
Pot Life 4.00 min

@Temperature 23.9 °C
4.00 min

@Temperature 75.0 °F