Polymer Property : Shear Strength = 319 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 2.20 MPa

@Temperature 82.0 °C
319 psi

@Temperature 180 °F
ASTM D1002-64
3M Scotch-Weld™ DP-605NS Off-White Adhesive in Duo-Pak Cartridges  (discontinued **)
Features include fast cure adhesive, semi-rigid urethane, 15-20 minutes handling strength, and excellent gap filler and non sag product for wood and plastic. Mix ratio by volume 1:1. Average T-Peel..