Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotch-Weld™ DP8805NS Low Odor Acrylic Adhesives

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ DP8805NS Low Odor Acrylic Adhesives.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Low Odor Acrylic Adhesives are high performance, two-part acrylic adhesives with lower odor than most acrylic adhesives. These toughened products offer excellent shear, peel, and impact performance. They provide improved adhesion to many plastics and metals, including those with slightly oily surfaces. These durable products feature an exceptionally fast rate of strength build, providing structural strength in minutes.Information provided by 3M
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Accelerator
1.13 g/cc
0.0408 lb/in³
Base
Viscosity 25000 cP
25000 cP
Accelerator
80000 cP
80000 cP
Base
Mechanical Properties Metric English Comments
Shear Strength 4.14 MPa
600 psi
Overlap, Polycarbonate, Adhesive/Cohesive Failure
7.58 MPa
1100 psi
Overlap, Acrylic, Substrate Failure
8.96 MPa
1300 psi
Overlap, ABS, Substrate Failure
12.4 MPa
1800 psi
Overlap, PVC, Substrate Failure
24.1 MPa
3500 psi
Overlap, Aluminum, Cohesive Failure