Material Notes:
3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI Gel (formerly SB09) is a fast curing, very high viscosity, gap filling cyanoacrylate. Its gel formation can be used for bonding poorly mating components and for porous substrates such as china and other ceramics and can be used on vertical surface as it will not drip or slump.Information provided by 3M
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Uncured
Brookfield Viscosity 7000 - 20000 cP
7000 - 20000 cP
RVT 'T-spindle' C @ 20 rpm
50000 - 90000 cP
50000 - 90000 cP
RVT 'T-spindle' C @ 2.5 rpm
Mechanical Properties Metric English Comments
Shear Strength 20.0 MPa
2900 psi
cured; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.500 - 1.00 min
0.00833 - 0.0167 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid