Material Notes:
3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI40 (formerly SB95) is a low viscosity surface insensitive ayanoacrylate that is used where very fast cure speed is desired. It is recommended for use on close-fitting parts and smooth even surfaces. It has been tested and passed the requirements of Commercial Item Description A-A-3097, Type II, Class 1 (formerly MIL-A-46050C).Information provided by 3M
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Uncured
Viscosity 34 - 44 cP
34 - 44 cP
ISO 3104/3105
Mechanical Properties Metric English Comments
Shear Strength 17.2 MPa
2500 psi
cured; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.0333 - 0.333 min
0.000555 - 0.00555 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid